Fluidized roasting reduction kinetics of low-grade pyrolusite coupling with pretreatment of stone coal

查看详情 浏览次数:2
单位1School of Civil and Environmental Engineering, University of Science and Technology Beijing;2State Key Laboratory of Biochemical Engineering, Institute of Process Engineering, Chinese Academy of Sciences收起
来源矿物冶金与材料学报(英文版)
出版年2013
期号第3期
摘要
Based on the fluidized roasting reduction technology of low-grade pyrolusite coupling with pretreatment of stone coal, the manganese reduction efficiency was investigated and technical conditions were optimized. It is found that the optimum manganese reduction efficiency can be up to 98.97% under the conditions that the mass ratio of stone coal to pyrolusite is 3:1, the roasting temperature of stone coal is 1000℃, the roasting temperature of pyrolusite is 800℃, and the roasting time is 2 h. Other low-grade pyrolusite ores in China from Guangxi, Hunan, and Guizhou Provinces were tested and all these minerals responded well, giving~99% manganese reduction efficiency. Meanwhile, the reduction kinetic model has been established. It is confirmed that the reduction process is controlled by the interface chemical reaction. The apparent activation energy is 36.397 kJ/mol.

@ 2023 版权所有 中国地质图书馆 (中国地质调查局地学文献中心)

京ICP备 05064591号 京公网安备11010802017129号

建议浏览器: 火狐、谷歌、微软 Edge、不支持 IE